#1 | ||
DIY Tragic
Join Date: Apr 2018
Location: Sydney, more than not. I hate it.
Posts: 23,950
|
I’m all but done with finishing up some brackets fabricated late last year by Slowsnake’s mate. Trimmed, drilled, tapped, edges broken… I want a simple protective clear matte anodising to stop them going “floury”. Anyone here had relatively recent dealings with a small works friendly anodiser?
|
||
![]() |
![]() ![]() |
![]() |
#2 | ||
DIY Tragic
Join Date: Apr 2018
Location: Sydney, more than not. I hate it.
Posts: 23,950
|
Another monologue.
![]() Looks like Barry Ave Mortdale is still the go, haven’t been there since about 2007 but had a chat with their office (Vicki) and happy to deal with mug punters. Minimum charge $70+ now. |
||
![]() |
![]() ![]() |
This user likes this post: |
![]() |
#3 | ||
DIY Tragic
Join Date: Apr 2018
Location: Sydney, more than not. I hate it.
Posts: 23,950
|
Very thorough assessment of my submitted parts, I was cautioned liberally that the weld filler rod’s composition may cause discolouration if more than a hint of silicon or magnesium is in there. Estimated lead time on drop-ins, is around two weeks, possibly less.
|
||
![]() |
![]() ![]() |
2 users like this post: |
![]() |
#4 | ||
DIY Tragic
Join Date: Apr 2018
Location: Sydney, more than not. I hate it.
Posts: 23,950
|
To wrap:
Parts dropped off 13/7, prepped for shop processes. Ready for pick-up 19/7. That’s a good turnaround. My only regret - if you could call it so - was opting for a matte finish instead of semi-shiny. It’s slightly darker than surrounding bits of anodised aluminium. I would go back; recommend them happily. The only thing I would do differently another time is bring in a finish sample, to be better guided on which process best matches. |
||
![]() |
![]() ![]() |